White powder on brick: what efflorescence is and what it means

What the white powder on brick is, where its salts and water come from, when it points to a moisture problem, and the gentle cleaning official guides describe.

Updated November 25, 2026 · 5 official sources
On this page: 5 sections
  1. 1What is the white chalky substance on my brick?
  2. 2What causes efflorescence in bricks?
  3. 3Should I be worried about efflorescence?
  4. 4How do you remove white efflorescence from bricks?
  5. 5Can cleaning or chemicals cause efflorescence?

The white powder on brick is efflorescence: a white powder or stain on the surface of the brick that results from water seeping through the brick and depositing salts.1 Water dissolves salts in the mortar, the brick or both, carries the salts to the surface of the wall and deposits them when the water evaporates.2

What is the white chalky substance on my brick?

Efflorescence is the accumulation of salts, usually sulphates, upon the outer surface of a wall of a building.2 The National Park Service's masonry glossary describes efflorescence as a whitish haze of soluble salts on masonry.3 The Park Service's brief on cleaning masonry calls efflorescence a powdery, white substance.4 The City of Burlington, Vermont's brick guide defines efflorescence as a white powder or stain on the surface of the brick that results from water seeping through the brick and depositing salts.1

Efflorescence appears only on the face brick, yet any material in a wall, from front to back and including the backing-up materials, may contribute to the salts on the outer surface.2

What causes efflorescence in bricks?

Two things have to be true for efflorescence to develop on a wall: the wall must be permeable to water, and the salts in the wall's materials must be soluble. Water that enters the wall dissolves any soluble salts, and the solution is then gradually carried outward to the exterior surface as evaporation proceeds.2

Water may enter a wall and be forced upward by capillarity from the soil, or water may enter in the form of rain, melted snow or direct absorption from humid air. Water added to the mortar materials at the time of mixing may also permeate a considerable portion of the wall.2

The salts may exist in the mortar, in the brick or in both materials.2 The National Park Service's glossary lists where the salts behind efflorescence come from:3

Source of the salts How the salts reach the brick
The brick itself Sulfates resulting from the curing and firing process are a common source of efflorescence in brick.
The ground Capillary action may pull soluble salts from the ground into the masonry, such as chlorides from salting of streets and sidewalks in winter and nitrates from fertilizers.
Lime mortar and the air Carbonates from lime mortar and airborne or water-deposited pollutants in the atmosphere may cause sulfates to be deposited on the surface of the masonry.
Chemical cleaning Efflorescence may be a combined salt residue left on the masonry surface by chemical cleaning, too strong a chemical solution or improper rinsing.

De-icing salts used near a building that have dissolved can also migrate into the masonry.4

Should I be worried about efflorescence?

Efflorescence itself may be more unsightly than harmful, but its presence on an older or historic masonry building often serves as a warning that water has found a point of entry into the structure. Once water has found a point of entry, more serious damage can usually be predicted.3

Efflorescence may also indicate subflorescence, which is salt accumulating under the surface of the masonry, and salt accumulations under the surface are potentially damaging to the masonry.3 Expansion of salts is one of the problems the National Park Service lists as a cause of cracking in brick masonry.5

In Burlington's guide, loose or discolored bricks can be an indication of a larger problem because the condition means there is moisture within or behind the brick, and problems with the roof, cornice or eave trim may be the cause. Staining on brick is usually telling of a larger problem, the same Burlington guide adds.1 Exposed masonry should be inspected periodically for cracking, spalling, bowing, sweeping, leaning and mortar deterioration.5 A spall is a small fragment removed from the face of the brick by a blow or inappropriate cleaning.1

How do you remove white efflorescence from bricks?

The National Park Service's glossary points to two preservation treatments for efflorescence: poulticing and water washing.3 Burlington's guide recommends water as a gentle method for cleaning the surface of brick, and low pressure water cleaning is often effective and safe for the brick and the environment.1

For historic masonry, the Park Service's recommended way to begin water washing is a very low pressure of 100 psi or below, even using a garden hose, progressing as needed to slightly higher pressure that is generally no higher than 300 to 400 psi. Water at too high a pressure can easily etch some types of brick.4

Three cautions come with water cleaning:

  • Check the wall first. Before a water cleaning project, all mortar joints should be sound and the building watertight, because otherwise water can seep through the walls to the interior.4
  • Stay out of cold weather. Any cleaning method involving water should never be done in cold weather or where frost or freezing is likely, because water within the masonry can freeze and cause spalling and cracking.4
  • Allow drying time. A masonry wall may take over a week to dry after cleaning.4

Can cleaning or chemicals cause efflorescence?

Cleaning may draw salts already in the masonry to the surface, where the salts will appear as efflorescence that may require a second treatment to be removed.4 Chemical cleaning can also leave salts of its own: efflorescence may be a combined salt residue left on the masonry surface by chemical cleaning, too strong a chemical solution or improper rinsing.3

Alkaline cleaners can deposit potentially damaging salts in the masonry.4 Brick cleaning is typically divided into three categories in Burlington's guide: water, chemical, and mechanical-abrasive cleaning.1

The National Park Service, the National Bureau of Standards and the City of Burlington, Vermont, checked November 2026.

Sources (5)

  1. City of Burlington, Vermont: Brick, Common Terms, read November 25, 2026 ↑
  2. National Bureau of Standards: Kiln and Dry-House Scum and Efflorescence, read November 25, 2026 ↑
  3. National Park Service: masonry deterioration glossary, Efflorescence, read November 25, 2026 ↑
  4. National Park Service: Preservation Brief 1, cleaning masonry, read November 25, 2026 ↑
  5. National Park Service: Common Problems with Brick Masonry, read November 25, 2026 ↑