Can you pressure wash or sandblast brick?

Why sandblasting damages brick, what water pressure preservation guidance treats as low enough, why a test patch comes first and when not to wet-clean.

Updated November 25, 2026 · 6 official sources
On this page: 5 sections
  1. 1Why does sandblasting damage brick?
  2. 2Can you pressure wash brick?
  3. 3What water pressure is low enough for brick?
  4. 4Why do a gentle method and a test patch come first?
  5. 5When should you not wet-clean brick?

Sandblasting damages brick: abrasive methods remove the hard, outer protective surface and make the brick more susceptible to rapid weathering and deterioration.1 Historic brick can be washed with water at low pressure, starting at 100 psi or below and generally going no higher than 300 to 400 psi.2

Why does sandblasting damage brick?

Abrasive cleaning is cleaning that works by eroding dirt or paint, and abrasive methods also tend to erode the surface of the building material at the same time. On brick, abrasive methods remove the hard, outer protective surface, which makes the brick more susceptible to rapid weathering and deterioration. Grit blasting may also increase the water permeability of a brick wall, because the impact of the grit particles tends to erode the bond between the mortar and the brick, leaving cracks or enlarging existing cracks where water can enter.1

Sound mortar joints can be worn away by abrasive techniques. Where one of two brick rowhouses with a common facade was sandblasted, the blasting removed the outer surface, left that brickwork rough and pitted, and removed a considerable portion of the mortar from the joints.1

Northfield's guidebook for its downtown historic district says brick and masonry should never be sandblasted, because sandblasting removes the hard surface of the brick and exposes the softer interior to moisture and deterioration.3 The City of Alexandria's guideline for its Old and Historic District lists abrasive cleaning that includes sandblasting as inappropriate.4 In Phoenix, the city's historic preservation guidance on graffiti says abrasive cleaners and sandblasting can cause brick and mortar damage on a historic building.5

Can you pressure wash brick?

Washing with low-pressure or medium-pressure water is probably a commonly used method for removing dirt or other pollutant soiling from historic masonry buildings. Using water at too high a pressure is a practice common to power washing and water blasting that is very abrasive and can easily etch marble and other soft stones as well as some types of brick.2 Alexandria's guideline for its Old and Historic District lists high pressure powerwashing as inappropriate beside sandblasting.4

Most commercial pressure washing systems operate at significantly higher pressures than the ones the General Services Administration's specification for cleaning historic masonry recommends, and a pressure regulator may be needed to reduce the pressure.6 The distance of the nozzle from the masonry surface, the type of nozzle and the gallons per minute are also important variables in water cleaning. Grains of stone or sand in the cleaning effluent on the ground are an indication that the water pressure may be too high.2

What water pressure is low enough for brick?

Water pressure in these documents is given in pounds per square inch, written psi.6

Guidance Use Pressure Source
National Park Service, Preservation Brief 1 Water washing Start at 100 psi or below, then generally no higher than 300 to 400 psi 2
General Services Administration specification Water washing Low jet pressure not to exceed 300 psi, with the psi to be determined during a mockup with GSA Historic Preservation approval 6
General Services Administration specification Rinsing after cleaning Start at 100 psi or below, no higher than 400 psi with minimal saturation, with the psi as determined during a mockup and approved by GSA Historic Preservation 6
City of Phoenix historic preservation guidance Water rinse after a paint remover Low to medium, no higher than 300 psi 5

The General Services Administration's specification says the "lowest possible pressure will be used to achieve desired results", and the optimal water pressure and wand distance are determined during cleaning test patches.6 National Park Service guidance starts at a very low pressure of 100 psi or below, even with a garden hose, and progresses as needed to slightly higher pressure. Scrubbing with natural bristle or synthetic bristle brushes can help in areas that are especially dirty, while metal brushes can abrade the surface and leave metal particles that can stain the masonry.2 In Phoenix, where a paint remover on a historic building requires a water rinse, a low to medium pressure rinse of no higher than 300 psi is encouraged to avoid water pressure induced damage to brick surfaces.5

Why do a gentle method and a test patch come first?

Even water-based methods can be damaging to historic masonry.2 The General Services Administration's specification reads "The gentlest cleaning methods should be tried first. The gentlest method for masonry is water and soft bristle brushes.".6 Testing should always begin with what Preservation Brief 1 calls "the gentlest and least invasive method" and proceed gradually, if necessary, to more complicated methods.2 Northfield's guidebook gives one reason for the caution: some cleaning methods will damage brick for life.3

A test area may be as small as six square inches to begin, may eventually be expanded to a square yard or more, and should include several masonry units and mortar joints. Cleaning tests should be evaluated only after the masonry has dried completely. A waiting period of a full year would be ideal so the test patch sees a full range of seasons, and where a year isn't possible the test patch should weather for at least a month or two.2

When should you not wet-clean brick?

Any cleaning method involving water should never be done in cold weather or where there is any likelihood of frost or freezing, because water within the masonry can freeze and crack the masonry. A masonry wall may take over a week to dry after cleaning, so no water cleaning should be permitted for several days before the first average frost date, or even earlier if local forecasts predict cold weather.2 Preservation Brief 6 puts water cleaning in warm weather when there is no danger of frost for several months.1

Before a water cleaning project begins, all mortar joints should be sound and the building watertight, because otherwise water can seep through the walls to the interior and leave rusting metal anchors and stained and ruined plaster.2 Openings should be tightly covered and cracks or joints well pointed before water or another liquid cleaning agent is used on masonry, to avoid the danger of water penetrating the building's facade.1 Under the General Services Administration's specification for its own cleaning work, the contractor installs temporary sealants at window and door perimeters before cleaning starts where they're required to prevent leakage to the interior.6

The National Park Service's Preservation Briefs 1 and 6, GSA's historic masonry cleaning specification and preservation guidelines from Alexandria, Northfield and Phoenix, checked November 2026.

Sources (6)

  1. National Park Service: Preservation Brief 6, Problems of Abrasive Cleaning, read November 25, 2026 ↑
  2. National Park Service: Preservation Brief 1, Water Washing, read November 25, 2026 ↑
  3. City of Northfield: Northfield Downtown Historic District Guidebook, Brick and Masonry, read November 25, 2026 ↑
  4. City of Alexandria: Masonry, Old and Historic District, read November 25, 2026 ↑
  5. City of Phoenix: Historic Preservation, read November 25, 2026 ↑
  6. US General Services Administration: Cleaning historic masonry, read November 25, 2026 ↑